Skip to main navigation Skip to search Skip to main content

Atomic Layer Deposition-Modified Bifunctional Electrocatalysts for Rechargeable Zinc-Air Batteries: Boosting Activity and Cycle Life

  • Fang Dong
  • , Zhangsen Chen
  • , Ning Chen
  • , Gaixia Zhang
  • , Shuhui Sun
  • Institut national de la recherche scientifique
  • University of Saskatchewan

Research output: Contribution to journal › Journal Article › peer-review

21 Citations (Scopus)

Abstract

The integration of transition metal-carbon composites has shown remarkable potential in achieving superior bifunctional electrocatalytic activity and robust stability in rechargeable zinc-air batteries (ZABs), primarily through electronic structure modulation and strategic structural design. While significant research is dedicated to the initial structure and performance of bifunctional electrocatalysts for rechargeable ZABs, their dynamic evolution during charge–discharge cycling remains underexplored. In this study, CoFe nanoparticles are encapsulated within carbon nanotubes co-doped with nitrogen and phosphorus (NPC) to mitigate dissolution and erosion risks. Further, the catalyst surface (CoFe-NPC) is precisely modified with a thin layer of nickel oxide (NiO) via atomic layer deposition (ALD), forming a protective layer with catalytic activity. The resulting ALD-modified catalyst, CoFe-NPC@NiO, exhibits outstanding bifunctional performance (ΔE = 0.592 V) for the oxygen reduction reaction (ORR) and oxygen evolution reaction (OER). Notably, the liquid flow ZAB using the CoFe-NPC@NiO cathode demonstrates exceptional rechargeable stability (2700 h, ≈4 months). Theoretical calculations and in situ X-ray absorption spectroscopy (XAS) analyses reveal that NiO modification significantly enhances both the catalytic activity and stability of the electrocatalyst. This work will provide valuable insights into the design of advanced electrocatalysts, facilitating advancements in activity enhancement, stability improvement, and selectivity optimization.

Original languageEnglish
Article number2502074
JournalAdvanced Energy Materials
Volume16
Issue number8
DOIs
Publication statusPublished - 25 Feb 2026

UN SDGs

This output contributes to the following UN Sustainable Development Goals (SDGs)

  1. SDG 7 - Affordable and Clean Energy
    SDG 7 Affordable and Clean Energy

!!!Keywords

  • atomic layer deposition
  • bifunctional electrocatalysts
  • in situ observation
  • zinc-air batteries

Fingerprint

Dive into the research topics of 'Atomic Layer Deposition-Modified Bifunctional Electrocatalysts for Rechargeable Zinc-Air Batteries: Boosting Activity and Cycle Life'. These topics are generated from the title and abstract of the publication. Together, they form a unique fingerprint.

Cite this