N2 - An experimental study was performed to determine the effects of temperature on the mechanical strength of resistance-welded quasi-isotropic carbon fiber reinforced polyphenylene sulfide (CF/PPS) composite joints. The resistance welding process was used to assemble the joints with a stainless steel mesh heating element (HE). A room temperature lap shear strength (LSS) of 28.47 MPa was obtained. The effects of temperature on the strength was assessed by testing the welded joints at temperatures of 21 °C, 62 °C, 82 °C, 90 °C, 118 °C and 150 °C, corresponding to aerospace standard test temperatures and temperatures near the glass transition of the PPS matrix. The LSS decreased with an increasing temperature with a larger drop in the vicinity of the glass transition temperature (Tg). The fracture surfaces of the joints revealed a failure mode changing from cohesive in the HE to cohesive with the HE remaining on one laminate only between room temperature and 62 °C. A third cohesive failure mode between the HE and the matrix was obtained at temperatures higher than Tg. At 118 °C, the failure mode was mostly HE disbonding and the mechanical strength was reduced by 49.8 %.
AB - An experimental study was performed to determine the effects of temperature on the mechanical strength of resistance-welded quasi-isotropic carbon fiber reinforced polyphenylene sulfide (CF/PPS) composite joints. The resistance welding process was used to assemble the joints with a stainless steel mesh heating element (HE). A room temperature lap shear strength (LSS) of 28.47 MPa was obtained. The effects of temperature on the strength was assessed by testing the welded joints at temperatures of 21 °C, 62 °C, 82 °C, 90 °C, 118 °C and 150 °C, corresponding to aerospace standard test temperatures and temperatures near the glass transition of the PPS matrix. The LSS decreased with an increasing temperature with a larger drop in the vicinity of the glass transition temperature (Tg). The fracture surfaces of the joints revealed a failure mode changing from cohesive in the HE to cohesive with the HE remaining on one laminate only between room temperature and 62 °C. A third cohesive failure mode between the HE and the matrix was obtained at temperatures higher than Tg. At 118 °C, the failure mode was mostly HE disbonding and the mechanical strength was reduced by 49.8 %.
UR - https://www.scopus.com/pages/publications/85050407920
M3 - Contribution to conference proceedings
AN - SCOPUS:85050407920
T3 - International SAMPE Technical Conference
BT - SAMPE Long Beach 2018 Conference and Exhibition
A2 - Storage, Kara
A2 - Sutter, Thomas
A2 - Beckwith, Scott
A2 - Bond, Gary
A2 - Storage, Tara
PB - Soc. for the Advancement of Material and Process Engineering
T2 - SAMPE Long Beach 2018 Conference and Exhibition
Y2 - 21 May 2018 through 24 May 2018
ER -