The laser powder bed fusion parameters were determined for a novel biomedical Ti-18Zr-14Nb (at%) alloy using both analytical and experimental approaches. An analytical model was used to calculate the laser powder bed fusion parameters such as laser power, scanning speed and hatching space providing the energy density on the powder bed surface ranging from 9 to 85 J/mm3, and the build rate – from 12 to 52 cm3/h. A technological processing window corresponding to a 25–45 J/mm3 energy density range and a 10–25 cm3/h build rate range is recommended for the fabrication of the fully dense Ti-18Zr-14Nb alloy with improved surface roughness.

Original languageEnglish
Pages (from-to)821-829
Number of pages9
JournalJournal of Materials Processing Technology
Volume252
DOIs
Publication statusPublished - Feb 2018

UN SDGs

This output contributes to the following UN Sustainable Development Goals (SDGs)

  1. SDG 9 - Industry, Innovation, and Infrastructure
    SDG 9 Industry, Innovation, and Infrastructure

Keywords

  • Additive manufacturing
  • Biocompatible superelastic alloy
  • Laser powder bed fusion
  • Processing parameters
  • Selective laser melting
  • Ti-based alloy

ASJC Scopus subject areas

  • Ceramics and Composites
  • Computer Science Applications
  • Metals and Alloys
  • Industrial and Manufacturing Engineering

Fingerprint

Dive into the research topics of 'New biocompatible near-beta Ti-Zr-Nb alloy processed by laser powder bed fusion: Process optimization'. These topics are generated from the title and abstract of the publication. Together, they form a unique fingerprint.

Cite this