Rational Design of Novel Catalysts with Atomic Layer Deposition for the Reduction of Carbon Dioxide

  • Zhangsen Chen
  • , Gaixia Zhang
  • , Jai Prakash
  • , Yi Zheng
  • , Shuhui Sun
  • Institut national de la recherche scientifique
  • National Institute of Technology Hamirpur
  • Fuzhou University

Research output: Contribution to journal › Review Article › peer-review

73 Citations (Scopus)

Fingerprint

Dive into the research topics of 'Rational Design of Novel Catalysts with Atomic Layer Deposition for the Reduction of Carbon Dioxide'. Together they form a unique fingerprint.
Sort by

Keyphrases

Chemical Engineering