Abstract

Laser Powder Bed Fusion (LPBF) is a predominant Additive Manufacturing (AM) process. While metallic LPBF is gaining popularity, one of the barriers facing its wider industrial use is the current relatively limited knowledge with respect to its dimensional and geometrical performance, as well as the inability to predict it. This paper presents an experimental investigation of the geometrical and dimensional deviations of selected LPBF-manufactured components according to the ASME Y14.5 (2009) standard. In this study, two types of axisymmetric parts (cylinder and cylindrical pyramid) were designed with three different levels of material concentration, and replicated at three different scales for a total of 18 test artifacts. These parts were manufactured from AlSi10Mg powder using an EOSINT M280 printer, subjected to stress relief annealing at 300 ◦C for two hours, removed from the platform and finished by micro shot peening. A complete statistical analysis was carried out on the artifacts before and after each post-processing step. The results of this investigation allowed for the quantification of the intra- (same part) and inter- (different parts) scale effects, as well as of the material concentration, stress relief, part removal and micro shot peening effects on the overall three-dimensional (3D) profile deviations and on the dimensional deviations of some selected features (e.g., diameter, thickness). For example, cylindrical pyramid parts showed the following average deviations of their outside diameters: a −63 µm shrinkage of the as-built part diameter as compared to its computer-assisted design (CAD) value, a +20 µm expansion after stress relief annealing as compared to the precedent step, a −18 µm shrinkage after part removal and, finally, a −50 µm shrinkage after micro shot peening.

Original languageEnglish
Article number49
JournalJournal of Manufacturing and Materials Processing
Volume3
Issue number2
DOIs
Publication statusPublished - Jun 2019

UN SDGs

This output contributes to the following UN Sustainable Development Goals (SDGs)

  1. SDG 9 - Industry, Innovation, and Infrastructure
    SDG 9 Industry, Innovation, and Infrastructure

Keywords

  • Additive manufacturing
  • Geometrical dimensioning
  • Laser powder bed fusion
  • Material concentration
  • Metrology
  • Post-processing
  • Selective laser melting
  • Tolerancing

ASJC Scopus subject areas

  • Mechanics of Materials
  • Mechanical Engineering
  • Industrial and Manufacturing Engineering

Fingerprint

Dive into the research topics of 'Scale, material concentration, stress relief and part removal effects on the dimensional behaviour of selected AlSi10Mg components manufactured by laser powder bed fusion'. These topics are generated from the title and abstract of the publication. Together, they form a unique fingerprint.

Cite this