T1 - Structure and properties features of nanostructured Ti-Ni SMA after severe plastic deformation and post-deformation annealing
AU - Brailovski, V.
AU - Inaekyan, K.
AU - Prokoshkin, S.
AU - Korotitskiy, A.
AU - Glezer, A.
PY - 2008
Y1 - 2008
N2 - Ti-50.0, Ti-50.26 and Ti-50.6at%Ni shape memory alloys are subjected to Cold Rolling (CR), with true strains varying from moderate (e=0.3) to severe (e=l.5-2.1) and High Pressure Torsion (HPT), with true strains varying from e=3.16 to 6.16. The study of the material thermal stability and mechanical properties is performed using DSC, microhardness and tensile testing techniques. CR with true strains higher than 0.5 initiates grain refinement and austenite amorphization, and the higher the cold work strain, the higher the grain refinement and the degree of amorphization, and the higher the ultimate strength, microhardness and Young's modulus of the material. It is shown that CR and HPT-processed Ti-Ni alloys are strongly heterogeneous materials containing amorphous matrix with embedded nanocrystals. The fraction of the amorphous phase in these materials cannot therefore be evaluated through the DSC technique because exothermal peaks measured contain inseparable contributions from both crystallization and grain growth phenomena. In the framework of the Johnson-Mehl-Avrami isothermal analysis, it is shown that for the CR-processed material (e =2), the Avrami exponent n = 1.25, which corresponds to annealing by grain growth-dominated mechanisms, whereas for the HPT-processed material (e = 6), n = 2.6, which corresponds to annealing by nucleation-and-grain growth mechanisms.
AB - Ti-50.0, Ti-50.26 and Ti-50.6at%Ni shape memory alloys are subjected to Cold Rolling (CR), with true strains varying from moderate (e=0.3) to severe (e=l.5-2.1) and High Pressure Torsion (HPT), with true strains varying from e=3.16 to 6.16. The study of the material thermal stability and mechanical properties is performed using DSC, microhardness and tensile testing techniques. CR with true strains higher than 0.5 initiates grain refinement and austenite amorphization, and the higher the cold work strain, the higher the grain refinement and the degree of amorphization, and the higher the ultimate strength, microhardness and Young's modulus of the material. It is shown that CR and HPT-processed Ti-Ni alloys are strongly heterogeneous materials containing amorphous matrix with embedded nanocrystals. The fraction of the amorphous phase in these materials cannot therefore be evaluated through the DSC technique because exothermal peaks measured contain inseparable contributions from both crystallization and grain growth phenomena. In the framework of the Johnson-Mehl-Avrami isothermal analysis, it is shown that for the CR-processed material (e =2), the Avrami exponent n = 1.25, which corresponds to annealing by grain growth-dominated mechanisms, whereas for the HPT-processed material (e = 6), n = 2.6, which corresponds to annealing by nucleation-and-grain growth mechanisms.
KW - Amorphous and nanocrystalline structures
KW - Severe plastic deformation
KW - Titanium-nickel shape memory alloys
UR - https://www.scopus.com/pages/publications/65649114756
U2 - 10.1361/cp2007smst017
DO - 10.1361/cp2007smst017
M3 - Contribution to conference proceedings
AN - SCOPUS:65649114756
SN - 9780871707222
T3 - SMST-2007 - Proceedings of the International Conference on Shape Memory and Superelastic Technologies
SP - 17
EP - 26
BT - SMST-2007 - Proceedings of the International Conference on Shape Memory and Superelastic Technologies
T2 - International Conference on Shape Memory and Superelastic Technologies, SMST-2007
Y2 - 2 December 2007 through 5 December 2007
ER -