TY - GEN
T1 - Dielectric design of LDPE properties
T2 - 2016 IEEE Conference on Electrical Insulation and Dielectric Phenomena, CEIDP 2016
AU - Fréchette, M. F.
AU - Veillette, R.
AU - Trudeau, M.
AU - Pirondelli, A.
AU - Fabiani, D.
AU - Anh, T. Tran
AU - Ghafarizadeh, B.
AU - David, E.
AU - El-Khoury, D.
AU - Castellon, J.
AU - Arinero, R.
N1 - Publisher Copyright:
© 2016 IEEE.
PY - 2016/12/15
Y1 - 2016/12/15
N2 - Low-density Polyethylene (LDPE) was modified by using simultaneously 2 additives. Each additive had a specific attribute. Silicon was used. Using TEM with EELS, it was proved first that the passivated version constituted a double core consisting of Si surrounded by a nanometric layer of amorphous Silica (SiO2). Thus Si brought the possibility of an enlarged dielectric storage capacity with a barrier controlling the electrical charge movement (via SiO2). Silicon was used in conjunction with Carbon Black (CB) and produced, upon some conditions, enlarged dielectric storage yet with intempestive conversion to a conducting state. At low voltage, LDPE containing 5 wt% CB and 3% or 0.25% Si remained insulating materials. During breakdown conditions with a 2 kV/s rise, only the composite containing 0.25 wt% CB and 3 wt% Si exhibited insulating conditions. These results draw attention to the importance of performing material system evaluation under dynamical conditions.
AB - Low-density Polyethylene (LDPE) was modified by using simultaneously 2 additives. Each additive had a specific attribute. Silicon was used. Using TEM with EELS, it was proved first that the passivated version constituted a double core consisting of Si surrounded by a nanometric layer of amorphous Silica (SiO2). Thus Si brought the possibility of an enlarged dielectric storage capacity with a barrier controlling the electrical charge movement (via SiO2). Silicon was used in conjunction with Carbon Black (CB) and produced, upon some conditions, enlarged dielectric storage yet with intempestive conversion to a conducting state. At low voltage, LDPE containing 5 wt% CB and 3% or 0.25% Si remained insulating materials. During breakdown conditions with a 2 kV/s rise, only the composite containing 0.25 wt% CB and 3 wt% Si exhibited insulating conditions. These results draw attention to the importance of performing material system evaluation under dynamical conditions.
KW - AC conductivity
KW - Nanodielectric structures
KW - Polyethylene nanocomposites
KW - dielectric relaxation
KW - polarization
UR - https://www.scopus.com/pages/publications/85009816422
U2 - 10.1109/CEIDP.2016.7785471
DO - 10.1109/CEIDP.2016.7785471
M3 - Contribution to conference proceedings
AN - SCOPUS:85009816422
T3 - Annual Report - Conference on Electrical Insulation and Dielectric Phenomena, CEIDP
SP - 52
EP - 57
BT - 2016 IEEE Conference on Electrical Insulation and Dielectric Phenomena, CEIDP 2016
PB - Institute of Electrical and Electronics Engineers Inc.
Y2 - 16 October 2016 through 19 October 2016
ER -