Résumé
We have investigated both the large area excimer laser-induced deposition of W and its silicides on GaAs to form Thermally stable Schottky contacts, and the reduction of a Cu(I) compound for the deposition of Cu interconnects for Si microelectronics. Using a KrF excimer laser at 25 mJ / cm2 and a mixture of WF6, SiH4 and Ar, metallic W is deposited with an average growth rate of 1 Å/pulse. For Cu deposition, the reduction by H2 of the precursor Cu(hfac)(TMVS) under a KrF excimer laser illumination of 9 mJ/cm2 gives metallic Cu with a Cu/C ratio of 4.35. For both processes, possible deposition mechanisms are discussed in terms of gas phase and surface reactions.
| langue originale | Anglais |
|---|---|
| Pages (de - à) | 208-214 |
| Nombre de pages | 7 |
| journal | Applied Surface Science |
| Volume | 79-80 |
| Numéro de publication | C |
| Les DOIs | |
| état | Publié - 2 mai 1994 |
| Modification externe | Oui |
Classification disciplinaire ASJC Scopus
- Physique de la matière condensée
- Surfaces et interfaces
- Surfaces, revêtements et films
Empreinte digitale
Voici les principaux termes ou expressions associés à « Excimer laser-induced metallization for in situ processing on Si and GaAs ». Ces libellés thématiques sont générés à partir du titre et du résumé de la publication. Ensemble, ils forment une empreinte digitale unique.Citer cette ressource
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver