Résumé

Friction stir welding (FSWing) induces residual stresses and distortions in welded structures. Such residual stresses reduce the fatigue life of welded components, while the induced distortions prevent the welding of large or thin components. In the present study, needle peening was used to induce additional residual stresses in 2.3-mm thick (FSWed) aluminum alloy (AA) 2024-T3 sheets. This was done with the objective to counterbalance the welding-induced stresses and thus reduce the overall stresses and distortions. The needle peening process, which stems from shot peening, consists of hammering a surface using cylindrical spherical ended shots sliding back and forth in a treatment head. An instrumented needle peening machine was used to carry out peening on as-received (or bare) and bead-on-plate FSWed AA2024-T3 material. In both cases, the width of the peening area corresponded to that of a typical weld. The influence of the peening process parameters such as needle size, applied power and travel speed on the surface quality and magnitude of the induced distortions were evaluated. The results indicate that, by increasing the needle diameter from 1.2 mm to 2.0 mm, the peening-induced deflection on bare sheet material increased by an average value of 27% while the roughness average, Ra, decreased by an average value of 47%. It was also found that a surface finish qualitatively similar to that of conventional shot peening could be obtained by using appropriate needle peening trajectories. Finally, needle peening with an applied power of 10% was sufficient for eliminating 37% of the welding-induced transverse curvature and 82% of the welding-induced longitudinal curvature.

Langue originaleAnglais
titreTHERMEC 2009
rédacteurs en chefTara Chandra, Tara Chandra, Tara Chandra, N. Wanderka, N. Wanderka, N. Wanderka, Walter Reimers, Walter Reimers, Walter Reimers, M. Ionescu, M. Ionescu, M. Ionescu
EditeurTrans Tech Publications Ltd
Pages1203-1208
Nombre de pages6
ISBN (imprimé)0878492941, 9780878492947
Les DOIs
ÉtatPublié - 2010
Modification externeOui
Evénement6th International Conference on Processing and Manufacturing of Advanced Materials - THERMEC'2009 - Berlin, Allemagne
Durée: 25 août 2009 → 29 août 2009

Série de publications

NomMaterials Science Forum
Volume638-642
ISSN (imprimé)0255-5476
ISSN (Electronique)1662-9752

Conférence

Conférence6th International Conference on Processing and Manufacturing of Advanced Materials - THERMEC'2009
Pays/TerritoireAllemagne
La villeBerlin
Période25/08/09 → 29/08/09

Classification disciplinaire ASJC Scopus

  • Sciences générales des matériaux
  • Physique de la matière condensée
  • Mécanique des matériaux
  • Ingénierie mécanique

Empreinte digitale

Voici les principaux termes ou expressions associés à « Limitation of distortion in friction stir welded (FSW) panels using needle peening ». Ces libellés thématiques sont générés à partir du titre et du résumé de la publication. Ensemble, ils forment une empreinte digitale unique.

Citer cette ressource