Machining/machinability of Rene 65 superalloy for aerospace applications

  • École de technologie supérieure

Résultats de recherche: Chapitre dans un livre, rapport, actes de conférence › Participation à un ouvrage collectif lié à un colloque ou une conférence › Revue par des pairs

4 Citations (Scopus)

Résumé

Rene 65 is a newly developed nickel-based superalloy, introduced in production of jet engine disks and blades. In comparison with existing cast and wrought nickel superalloys, Rene 65 possesses improved thermo-mechanical loading properties such as; reduced cyclic fatigue, crack growth strength, creep rupture resistance, and greater ultimate yield tensile strengths. However, its behaviour during machining is still an on-going area of research. This study evaluates the machinability of this new superalloy during drilling and milling operations. Experimental cutting tests were conducted on Rene 65 to establish the machining challenges this superalloy faces. Cutting forces, tool wear and surface roughness were used to assess its machinability. The response surface method (RSM) was used to optimize the machining parameters in order to improve the machining conditions.

langue originaleAnglais
titreProceedings of 2020 IEEE 11th International Conference on Mechanical and Intelligent Manufacturing Technologies, ICMIMT 2020
EditeurInstitute of Electrical and Electronics Engineers Inc.
Pages1-7
Nombre de pages7
ISBN (Electronique)9781728153322
Les DOIs
étatPublié - janv. 2020
Evénement11th IEEE International Conference on Mechanical and Intelligent Manufacturing Technologies, ICMIMT 2020 - Cape Town, Afrique du Sud
Durée: 20 janv. 2020 → 22 janv. 2020

Série de publications

NomProceedings of 2020 IEEE 11th International Conference on Mechanical and Intelligent Manufacturing Technologies, ICMIMT 2020

Conférence

Conférence11th IEEE International Conference on Mechanical and Intelligent Manufacturing Technologies, ICMIMT 2020
Pays/TerritoireAfrique du Sud
La villeCape Town
Période20/01/20 → 22/01/20

SDG des Nations Unies

Ce résultat contribue à ou aux Objectifs de développement durable suivants

  1. SDG 9 – Industrie, innovation et infrastructure
    SDG 9 – Industrie, innovation et infrastructure

Empreinte digitale

Voici les principaux termes ou expressions associés à « Machining/machinability of Rene 65 superalloy for aerospace applications ». Ces libellés thématiques sont générés à partir du titre et du résumé de la publication. Ensemble, ils forment une empreinte digitale unique.

Citer cette ressource