N2 - The Ti-21.8Nb-6Zr and Ti-19.7Nb-5.8Ta (at.%) shape memory alloys are thermomechanically treated by cold drawing and post-deformation annealing at 550-600°C forming a nanosubgrained structure in the β-phase. Cyclic mechanical testing using a "loading-unloading" mode with 2% tensile strain in each half-cycle reveals the non-perfect superelastic behavior of both alloys during the very first cycles of testing, which becomes perfect during further mechanocycling. The Young's modulus of thermomechanically-treated alloys is low (about 45 GPa), and it decreases during mechanocycling (n=10 cycles) down to 25-35 GPa, approaching the Young's modulus of cortical bone tissues. The Young's modulus obtained in the 10th cycle is stable or changes only slightly during a further 40-day pause at room temperature and then during repeated mechanocycling. The residual strain per cycle, the transformation yield stress and the mechanical hysteresis decrease during mechanocycling. Subsequent to a 40-day pause at room temperature, they restore their initial values. Repeated mechanocycling is accompanied by a repeated decrease of these parameters.
AB - The Ti-21.8Nb-6Zr and Ti-19.7Nb-5.8Ta (at.%) shape memory alloys are thermomechanically treated by cold drawing and post-deformation annealing at 550-600°C forming a nanosubgrained structure in the β-phase. Cyclic mechanical testing using a "loading-unloading" mode with 2% tensile strain in each half-cycle reveals the non-perfect superelastic behavior of both alloys during the very first cycles of testing, which becomes perfect during further mechanocycling. The Young's modulus of thermomechanically-treated alloys is low (about 45 GPa), and it decreases during mechanocycling (n=10 cycles) down to 25-35 GPa, approaching the Young's modulus of cortical bone tissues. The Young's modulus obtained in the 10th cycle is stable or changes only slightly during a further 40-day pause at room temperature and then during repeated mechanocycling. The residual strain per cycle, the transformation yield stress and the mechanical hysteresis decrease during mechanocycling. Subsequent to a 40-day pause at room temperature, they restore their initial values. Repeated mechanocycling is accompanied by a repeated decrease of these parameters.
KW - Functional
KW - SMA
KW - Superelasticity
KW - Thermomechanical treatment
KW - Titanium based alloys
UR - https://www.scopus.com/pages/publications/84874068826
U2 - 10.4028/www.scientific.net/MSF.738-739.481
DO - 10.4028/www.scientific.net/MSF.738-739.481
M3 - Contribution to conference proceedings
AN - SCOPUS:84874068826
SN - 9783037856109
T3 - Materials Science Forum
SP - 481
EP - 485
BT - European Symposium on Martensitic Transformations, ESOMAT 2012
A2 - Prokoshkin, Sergey
A2 - Resnina, Natalia
PB - Trans Tech Publications Ltd
T2 - 9th European Symposium on Martensitic Transformations, ESOMAT 2012
Y2 - 9 September 2012 through 16 September 2012
ER -