Polishing-assisted galvanic corrosion in the dissimilar friction stir welded joint of AZ31 magnesium alloy to 2024 aluminum alloy

  • C. Liu
  • , D. L. Chen
  • , S. Bhole
  • , X. Cao
  • , M. Jahazi
  • Toronto Metropolitan University
  • National Research Council of Canada

Résultats de recherche: Contribution à un journal › Article publié dans une revue, révisé par les pairs › Revue par des pairs

125 Citations (Scopus)

Résumé

Galvanic corrosion of a dissimilar friction stir welded 2024-T3 Al/AZ31B-H24 Mg joint prepared using a water-based and a non-water-based polishing solution was characterized. Microstructure and the distribution of chemical elements were analyzed using optical microscopy, scanning electron microscopy and energy dispersive X-ray spectroscopy. The stir zone polished using water-based solution was observed to be much more susceptible to galvanic corrosion attack than that obtained using non-water-based polishing solution. The location of corrosion attack was observed in the narrow regions of AZ31 Mg alloy adjacent to Al2024 regions in the stir zone. The occurrence of galvanic corrosion was due to the formation of Mg/Al galvanic couples with a small ratio of anode-to-cathode surface area. The corrosion product was primarily the porous magnesium hydroxide with characteristic microcracks and exhibited a low microhardness value.

langue originaleAnglais
Pages (de - à)370-376
Nombre de pages7
journalMaterials Characterization
Volume60
Numéro de publication5
Les DOIs
étatPublié - mai 2009
Modification externeOui

Classification disciplinaire ASJC Scopus

  • Sciences générales des matériaux
  • Physique de la matière condensée
  • Mécanique des matériaux
  • Ingénierie mécanique

Empreinte digitale

Voici les principaux termes ou expressions associés à « Polishing-assisted galvanic corrosion in the dissimilar friction stir welded joint of AZ31 magnesium alloy to 2024 aluminum alloy ». Ces libellés thématiques sont générés à partir du titre et du résumé de la publication. Ensemble, ils forment une empreinte digitale unique.

Citer cette ressource