TY - GEN
T1 - TEOS-PECVD films for high-quality SiO2 cladding layers in Si3N4-photonics with low mechanical stress and optical loss
AU - Mehrvar, Leila
AU - Le Drogoff, Boris
AU - Menard, Michael
AU - Chaker, Mohamed
N1 - Publisher Copyright:
© 2024 IEEE.
PY - 2024
Y1 - 2024
N2 - In this paper, we developed a multistep approach for depositing silicon dioxide (SiO2) cladding layers using TEOS-based PECVD. We deposited the SiO2 layer in multiple thin steps, separated by annealing time at 1000oC, to gradually increase the thickness and avoid cracking. Our results showed that the SiO2 films deposited under different processes had the same stress, and refractive index behavior, as long as the thickness of each step is below a critical thickness (500nm on Si substrate and 300nm on SiO2 substrate); hence, we were able to achieve high coverage and low mechanical stress (-200 MPa) in the deposited SiO2 films. RBS results demonstrated the high quality of our TEOS-based oxide without any contamination, contrary to the nitrogen contamination that exists through the whole thickness of the silane-based SiO2 films. To demonstrate the effectiveness of our TEOS-PECVD process, we integrated the SiO2 cladding layers with silicon nitride (Si3N4) waveguides and the stability of their optical responses at 1550 nm under various annealing steps was confirmed. Our results showed that the SiO2 cladding layers provided effective optical confinement, with optical losses around 0.67 dB/cm suitable for high-performance waveguides operating at 1550 nm.
AB - In this paper, we developed a multistep approach for depositing silicon dioxide (SiO2) cladding layers using TEOS-based PECVD. We deposited the SiO2 layer in multiple thin steps, separated by annealing time at 1000oC, to gradually increase the thickness and avoid cracking. Our results showed that the SiO2 films deposited under different processes had the same stress, and refractive index behavior, as long as the thickness of each step is below a critical thickness (500nm on Si substrate and 300nm on SiO2 substrate); hence, we were able to achieve high coverage and low mechanical stress (-200 MPa) in the deposited SiO2 films. RBS results demonstrated the high quality of our TEOS-based oxide without any contamination, contrary to the nitrogen contamination that exists through the whole thickness of the silane-based SiO2 films. To demonstrate the effectiveness of our TEOS-PECVD process, we integrated the SiO2 cladding layers with silicon nitride (Si3N4) waveguides and the stability of their optical responses at 1550 nm under various annealing steps was confirmed. Our results showed that the SiO2 cladding layers provided effective optical confinement, with optical losses around 0.67 dB/cm suitable for high-performance waveguides operating at 1550 nm.
KW - Annealing
KW - Mechanical residual stress
KW - Multistep deposition
KW - Propagation loss
KW - SiO top cladding
KW - TEOS-PECVD
UR - https://www.scopus.com/pages/publications/85202347983
U2 - 10.1109/PN62551.2024.10621767
DO - 10.1109/PN62551.2024.10621767
M3 - Contribution to conference proceedings
AN - SCOPUS:85202347983
T3 - 2024 Photonics North, PN 2024
BT - 2024 Photonics North, PN 2024
PB - Institute of Electrical and Electronics Engineers Inc.
T2 - 2024 Photonics North, PN 2024
Y2 - 28 May 2024 through 30 May 2024
ER -