Abstract
Metallic foams with porosity ranging from 0.25 to 0.65 have been produced from TiCp, TiNbZr and TiNbTa prealloyed powder by using the space-holder technique, and analysed from both the pore morphology and mechanical properties' points of view. For all the foams, the most suitable porosity range for bone ingrowth appears to be 0.35 to 0.45, since these porosities lead to a pore size that is globally encompassed in the recommended 100600 μmrange. From the mechanical behavior point of view, all of the as-sintered foams demonstrate similar compression behavior in terms of their apparent Young'smodulus and critical stresses. In the recommended 0.3 0.45 porosity range, their Young's modulus varies from 15 to 8 GPa, whilst their yield stress varies from 300 to 150 MPa. The first characteristic comes close to that of cortical bone, whilst the second significantly exceeds bone resistance. Compared to Ti foams, the mechanical properties of metastable TNZ and TNT alloy foams can also be regulatedwithin a±20% range, by selecting an appropriate post-sintering thermal treatment. This effect, which is initiated by activating reversible stress-induced β to α" martensitic transformation, is strongly perceptible for TNZ foams, whilst much less pronounced for TNT foams.
| Original language | English |
|---|---|
| Pages (from-to) | 421-433 |
| Number of pages | 13 |
| Journal | Materials Science and Engineering C |
| Volume | 45 |
| DOIs | |
| Publication status | Published - 1 Dec 2014 |
Keywords
- Metallic foams
- Metallography
- Powder metallurgy
- Shape memory
- X-ray diffraction
ASJC Scopus subject areas
- General Medicine
Fingerprint
Dive into the research topics of 'Fabrication, morphology and mechanical properties of Ti and metastable Ti-based alloy foams for biomedical applications'. These topics are generated from the title and abstract of the publication. Together, they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver