Metallic foams with porosity ranging from 0.25 to 0.65 have been produced from TiCp, TiNbZr and TiNbTa prealloyed powder by using the space-holder technique, and analysed from both the pore morphology and mechanical properties' points of view. For all the foams, the most suitable porosity range for bone ingrowth appears to be 0.35 to 0.45, since these porosities lead to a pore size that is globally encompassed in the recommended 100600 μmrange. From the mechanical behavior point of view, all of the as-sintered foams demonstrate similar compression behavior in terms of their apparent Young'smodulus and critical stresses. In the recommended 0.3 0.45 porosity range, their Young's modulus varies from 15 to 8 GPa, whilst their yield stress varies from 300 to 150 MPa. The first characteristic comes close to that of cortical bone, whilst the second significantly exceeds bone resistance. Compared to Ti foams, the mechanical properties of metastable TNZ and TNT alloy foams can also be regulatedwithin a±20% range, by selecting an appropriate post-sintering thermal treatment. This effect, which is initiated by activating reversible stress-induced β to α" martensitic transformation, is strongly perceptible for TNZ foams, whilst much less pronounced for TNT foams.
| Langue originale | Anglais |
|---|---|
| Pages (de - à) | 421-433 |
| Nombre de pages | 13 |
| Revue | Materials Science and Engineering C |
| Volume | 45 |
| Les DOIs | |
| État | Publié - 1 déc. 2014 |
Classification disciplinaire ASJC Scopus
- Médecine générale
Empreinte digitale
Voici les principaux termes ou expressions associés à « Fabrication, morphology and mechanical properties of Ti and metastable Ti-based alloy foams for biomedical applications ». Ces libellés thématiques sont générés à partir du titre et du résumé de la publication. Ensemble, ils forment une empreinte digitale unique.Citer cette ressource
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver