Skip to main navigation Skip to search Skip to main content

Friction stir welding of an aerospace magnesium alloy

  • National Research Council of Canada

Research output: Contribution to conference types › Conference Paper › peer-review

3 Citations (Scopus)

Abstract

Hot rolled AZ31B-H24 sheets with a thickness of 4.95 mm were joined using an MTS ISTIR friction stir welding machine. The cavity defects in the butt joints were studied and two mechanisms are observed. The pores are thought to be due to volume deficiency, and/or poor material flow and mixing. Excessive metal loss may cause subsurface pores which usually occur at the upper half of the welding nugget at the advancing side. Poor material flow and mixing may form internal pores which are usually elongated and curved, with the concave side in the welding direction. The grain size in the weld nugget was observed to be larger than that in the thermal-mechanically affected zone or heat-affected zone due to recrystallization, causing a drop in Vickers microindentation hardness.

Original languageEnglish
Pages213-222
Number of pages10
Publication statusPublished - 2007
Externally publishedYes
Event4th Symposium on Friction Stir Welding and Processing - Orlando, FL, United States
Duration: 25 Feb 2007 → 1 Mar 2007

Conference

Conference4th Symposium on Friction Stir Welding and Processing
Country/TerritoryUnited States
CityOrlando, FL
Period25/02/07 → 1/03/07

Keywords

  • Friction stir welding
  • Hardness
  • Magnesium alloy
  • Microstructure
  • Porosity

ASJC Scopus subject areas

  • Condensed Matter Physics
  • Mechanics of Materials
  • Metals and Alloys