Résumé
Hot rolled AZ31B-H24 sheets with a thickness of 4.95 mm were joined using an MTS ISTIR friction stir welding machine. The cavity defects in the butt joints were studied and two mechanisms are observed. The pores are thought to be due to volume deficiency, and/or poor material flow and mixing. Excessive metal loss may cause subsurface pores which usually occur at the upper half of the welding nugget at the advancing side. Poor material flow and mixing may form internal pores which are usually elongated and curved, with the concave side in the welding direction. The grain size in the weld nugget was observed to be larger than that in the thermal-mechanically affected zone or heat-affected zone due to recrystallization, causing a drop in Vickers microindentation hardness.
| Langue originale | Anglais |
|---|---|
| Pages | 213-222 |
| Nombre de pages | 10 |
| État | Publié - 2007 |
| Modification externe | Oui |
| Evénement | 4th Symposium on Friction Stir Welding and Processing - Orlando, FL, Etats-Unis Durée: 25 févr. 2007 → 1 mars 2007 |
Conférence
| Conférence | 4th Symposium on Friction Stir Welding and Processing |
|---|---|
| Pays/Territoire | Etats-Unis |
| La ville | Orlando, FL |
| Période | 25/02/07 → 1/03/07 |
Classification disciplinaire ASJC Scopus
- Physique de la matière condensée
- Mécanique des matériaux
- Métaux et alliages
Empreinte digitale
Voici les principaux termes ou expressions associés à « Friction stir welding of an aerospace magnesium alloy ». Ces libellés thématiques sont générés à partir du titre et du résumé de la publication. Ensemble, ils forment une empreinte digitale unique.Citer cette ressource
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver