Ti-50 at % Ni alloy wire is subjected to cold-rolling (true strain e=0.3-1.9) and post-deformation annealing (200-700°C range). For all levels of cold work, the maxima of recovery strain and stress are obtained after annealing in the 350-400°C range. For the moderately-to-high cold-worked material (e=0.3-0.88), this annealing leads to polygonization, while for the severely cold-worked one (e=1.9), to the material nanocrystallization (grains of 50-80 nm in size). Nanocrystallized alloy generates 30% higher recovery stresses (up to 1450 MPa) and 10% higher completely recoverable strains (more than 8 %) as compared to the polygonized alloy, while having comparable mechanical properties in tension.
| Original language | English |
|---|---|
| Journal | Journal of ASTM International |
| Volume | 3 |
| Issue number | 6 |
| DOIs | |
| Publication status | Published - 2006 |
Keywords
- Nanocrystalline structure
- Nickel-titanium shape memory alloys
- Post-deformation annealing
- Severe plastic deformation
ASJC Scopus subject areas
- Environmental Engineering
- General Materials Science
- Nuclear Energy and Engineering
- General Engineering
- Public Health, Environmental and Occupational Health
Fingerprint
Dive into the research topics of 'Functional properties of nanostructured Ti-50.0 at % Ni alloys'. These topics are generated from the title and abstract of the publication. Together, they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver