Résumé
Ti-50 at % Ni alloy wire is subjected to cold-rolling (true strain e=0.3-1.9) and post-deformation annealing (200-700°C range). For all levels of cold work, the maxima of recovery strain and stress are obtained after annealing in the 350-400°C range. For the moderately-to-high cold-worked material (e=0.3-0.88), this annealing leads to polygonization, while for the severely cold-worked one (e=1.9), to the material nanocrystallization (grains of 50-80 nm in size). Nanocrystallized alloy generates 30% higher recovery stresses (up to 1450 MPa) and 10% higher completely recoverable strains (more than 8 %) as compared to the polygonized alloy, while having comparable mechanical properties in tension.
| Langue originale | Anglais |
|---|---|
| Revue | Journal of ASTM International |
| Volume | 3 |
| Numéro de publication | 6 |
| Les DOIs | |
| État | Publié - 2006 |
Classification disciplinaire ASJC Scopus
- Ingénierie de l'environnement
- Sciences générales des matériaux
- Ingénierie et énergie nucléaire
- Ingénierie générale
- Santé publique, environnementale et au travail
Empreinte digitale
Voici les principaux termes ou expressions associés à « Functional properties of nanostructured Ti-50.0 at % Ni alloys ». Ces libellés thématiques sont générés à partir du titre et du résumé de la publication. Ensemble, ils forment une empreinte digitale unique.Citer cette ressource
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver