Skip to main navigation Skip to search Skip to main content

High temperature deformation of nickel base superalloy Udimet 520

  • A. R. Mashreghi
  • , H. Monajatizadeh
  • , M. Jahazi
  • , S. Yue
  • Tarbiat Modarres University
  • National Research Council of Canada
  • McGill University

Research output: Contribution to journal › Journal Article › peer-review

29 Citations (Scopus)

Abstract

The high temperature deformation behaviour of nickel base superalloy Udimet 520 was characterised using hot compression isothermal tests. Hot compression tests were conducted between 900 and 1150°C with strain rates of 0·001, 0·01, 0·1 and 1 s-1. Testing at ≤950°C led to sample fracture for all the applied strain rates. The flow behaviour at 1000, 1050 and 1075°C indicated the occurrence of dynamic recovery. For specimens tested at 1100, 1125 and 1150°C, recrystallisation is the softening mechanism. The strain rate sensitivity factor m was estimated for various thermomechanical histories. The activation energy for the hot deformation was determined to be 780 kJ mol1. The Zener-Hollomon parameter was also determined and its variation with grain size was studied with deformation conditions. The microstructures of all samples were examined by both optical and scanning electron microscopy. The presence and variations in the morphology and size distribution of deformed and recrystallised grains were determined and related to the deformation conditions.

Original languageEnglish
Pages (from-to)161-166
Number of pages6
JournalMaterials Science and Technology
Volume20
Issue number2
DOIs
Publication statusPublished - Feb 2004
Externally publishedYes

Keywords

  • Hot compression tests
  • Nickel base superalloys

ASJC Scopus subject areas

  • General Materials Science
  • Condensed Matter Physics
  • Mechanics of Materials
  • Mechanical Engineering

Fingerprint

Dive into the research topics of 'High temperature deformation of nickel base superalloy Udimet 520'. These topics are generated from the title and abstract of the publication. Together, they form a unique fingerprint.

Cite this