Passer à la navigation principale Passer à la recherche Passer au contenu principal

High temperature deformation of nickel base superalloy Udimet 520

  • A. R. Mashreghi
  • , H. Monajatizadeh
  • , M. Jahazi
  • , S. Yue
  • Tarbiat Modarres University
  • National Research Council of Canada
  • McGill University

Résultats de recherche: Contribution à un journal › Article publié dans une revue, révisé par les pairs › Revue par des pairs

29 Citations (Scopus)

Résumé

The high temperature deformation behaviour of nickel base superalloy Udimet 520 was characterised using hot compression isothermal tests. Hot compression tests were conducted between 900 and 1150°C with strain rates of 0·001, 0·01, 0·1 and 1 s-1. Testing at ≤950°C led to sample fracture for all the applied strain rates. The flow behaviour at 1000, 1050 and 1075°C indicated the occurrence of dynamic recovery. For specimens tested at 1100, 1125 and 1150°C, recrystallisation is the softening mechanism. The strain rate sensitivity factor m was estimated for various thermomechanical histories. The activation energy for the hot deformation was determined to be 780 kJ mol1. The Zener-Hollomon parameter was also determined and its variation with grain size was studied with deformation conditions. The microstructures of all samples were examined by both optical and scanning electron microscopy. The presence and variations in the morphology and size distribution of deformed and recrystallised grains were determined and related to the deformation conditions.

langue originaleAnglais
Pages (de - à)161-166
Nombre de pages6
journalMaterials Science and Technology
Volume20
Numéro de publication2
Les DOIs
étatPublié - févr. 2004
Modification externeOui

Classification disciplinaire ASJC Scopus

  • Sciences générales des matériaux
  • Physique de la matière condensée
  • Mécanique des matériaux
  • Ingénierie mécanique

Empreinte digitale

Voici les principaux termes ou expressions associés à « High temperature deformation of nickel base superalloy Udimet 520 ». Ces libellés thématiques sont générés à partir du titre et du résumé de la publication. Ensemble, ils forment une empreinte digitale unique.

Citer cette ressource