Abstract
This paper describes a successfully implemented method for controlling the chemical composition of Ti-Zr-Nb shape memory alloys for laser powder bed fusion (LPBF) printing of orthopedic implants. It is shown that to achieve the target Ti-18Zr-15Nb (at.%) composition in the printed product, the ingot composition must be adjusted by increasing the Ti content by 2.5 % while decreasing the Zr and Nb contents by 1% and 1.5%, respectively. These modifications compensate for compositional variations occurring during powder atomization and LPBF processing, and − following a post-fusion annealing at 550℃ for 30 min − result in a printed product with excellent room-temperature superelasticity: a superelastic recovery strain of 2.6% and a total recovery strain of 6.1%. The obtained mechanical properties of the material (an ultimate tensile strength of 725 MPa and Young's modulus of 53 GPa) make the LPBF-printed and annealed Ti-18Zr-15Nb alloy of this study a promising candidate for orthopedic implants.
| Original language | English |
|---|---|
| Article number | 138872 |
| Journal | Materials Letters |
| Volume | 398 |
| DOIs | |
| Publication status | Published - 1 Nov 2025 |
Keywords
- Chemical composition
- Laser powder bed fusion
- Structural-phase state
- Superelastic properties
- Ti-Zr-Nb shape memory alloy
ASJC Scopus subject areas
- General Materials Science
- Condensed Matter Physics
- Mechanics of Materials
- Mechanical Engineering
Fingerprint
Dive into the research topics of 'Improving superelasticity of a laser powder bed-fused Ti-Zr-Nb alloy via the ingot composition adjustments'. These topics are generated from the title and abstract of the publication. Together, they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver