Résumé
This paper describes a successfully implemented method for controlling the chemical composition of Ti-Zr-Nb shape memory alloys for laser powder bed fusion (LPBF) printing of orthopedic implants. It is shown that to achieve the target Ti-18Zr-15Nb (at.%) composition in the printed product, the ingot composition must be adjusted by increasing the Ti content by 2.5 % while decreasing the Zr and Nb contents by 1% and 1.5%, respectively. These modifications compensate for compositional variations occurring during powder atomization and LPBF processing, and − following a post-fusion annealing at 550℃ for 30 min − result in a printed product with excellent room-temperature superelasticity: a superelastic recovery strain of 2.6% and a total recovery strain of 6.1%. The obtained mechanical properties of the material (an ultimate tensile strength of 725 MPa and Young's modulus of 53 GPa) make the LPBF-printed and annealed Ti-18Zr-15Nb alloy of this study a promising candidate for orthopedic implants.
| langue originale | Anglais |
|---|---|
| Numéro d'article | 138872 |
| journal | Materials Letters |
| Volume | 398 |
| Les DOIs | |
| état | Publié - 1 nov. 2025 |
Classification disciplinaire ASJC Scopus
- Sciences générales des matériaux
- Physique de la matière condensée
- Mécanique des matériaux
- Ingénierie mécanique
Empreinte digitale
Voici les principaux termes ou expressions associés à « Improving superelasticity of a laser powder bed-fused Ti-Zr-Nb alloy via the ingot composition adjustments ». Ces libellés thématiques sont générés à partir du titre et du résumé de la publication. Ensemble, ils forment une empreinte digitale unique.Citer cette ressource
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver