TY - GEN
T1 - Thermal stability and nanocrystallization of amorphous Ti-Ni alloys prepared by cold rolling and post-deformation annealing
AU - Brailovski, V.
AU - Prokoshkin, S. D.
AU - Bastarash, E.
AU - Demers, V.
AU - Inaekyan, K. E.
AU - Khmelevskaya, I. Yu
PY - 2007
Y1 - 2007
N2 - The thermomechanical processing consisting in severe cold rolling (true strain 0.7-1.9) followed by a post-deformation annealing (200-700°C) is applied to Ti-50.0 and 50.7at%Ni alloys. The thermal stability of the amorphous phase as well as the influence of post-deformation annealing on the structure, substructure and temperature range of martensitic transformations are studied using TEM and DSC techniques. For a given level of cold work, the equiatomic alloy has a higher volume fraction of amorphous phase than the nickel-rich one. For both alloys, the higher the volume fraction of the amorphous phase, the higher the thermal stability. For a given post-deformation annealing temperature, the DSC martensitic transformation peaks from the material subjected to amorphization cold work are sharper and the hysteresis between the direct and reverse transformations is narrower than those for a material subjected to strain hardening cold work. This observation confirms the absence of the well-developed dislocation substructure in the severely deformed alloy subjected to nanocrystallization heat treatment, which is consistent with TEM results.
AB - The thermomechanical processing consisting in severe cold rolling (true strain 0.7-1.9) followed by a post-deformation annealing (200-700°C) is applied to Ti-50.0 and 50.7at%Ni alloys. The thermal stability of the amorphous phase as well as the influence of post-deformation annealing on the structure, substructure and temperature range of martensitic transformations are studied using TEM and DSC techniques. For a given level of cold work, the equiatomic alloy has a higher volume fraction of amorphous phase than the nickel-rich one. For both alloys, the higher the volume fraction of the amorphous phase, the higher the thermal stability. For a given post-deformation annealing temperature, the DSC martensitic transformation peaks from the material subjected to amorphization cold work are sharper and the hysteresis between the direct and reverse transformations is narrower than those for a material subjected to strain hardening cold work. This observation confirms the absence of the well-developed dislocation substructure in the severely deformed alloy subjected to nanocrystallization heat treatment, which is consistent with TEM results.
KW - Amorphous alloys
KW - Nanocrystalline structure
KW - Nickel-titanium shape memory alloys
KW - Post-deformation annealing
KW - Severe plastic deformation
KW - Thermomechanical processing
UR - https://www.scopus.com/pages/publications/38349016860
U2 - 10.4028/www.scientific.net/msf.539-543.1964
DO - 10.4028/www.scientific.net/msf.539-543.1964
M3 - Contribution to conference proceedings
AN - SCOPUS:38349016860
SN - 0878494286
SN - 9780878494286
T3 - Materials Science Forum
SP - 1964
EP - 1970
BT - Supplement to THERMEC 2006, 5th International Conference on PROCESSING and MANUFACTURING OF ADVANCED MATERIALS, THERMEC 2006
PB - Trans Tech Publications Ltd
T2 - 5th International Conference on Processing and Manufacturing of Advanced Materials - THERMEC'2006
Y2 - 4 July 2006 through 8 July 2006
ER -